聚丙烯(Broad MWD) |
|
|
|
|
|
货号 |
Mw |
Mn |
Mp |
IV* |
|
|
PP800K |
801,000 |
127,000 |
190,000 |
4.405 |
|
|
PP575K |
575,000 |
100,000 |
138,200 |
3.663 |
|
|
PP467K |
467,300 |
75,400 |
125,600 |
3.169 |
|
|
PP350K |
348,300 |
43,500 |
198,000 |
2.323 |
|
|
PP300K |
297,000 |
47,500 |
160,000 |
2.12 |
|
|
PP270K |
267,000 |
43,300 |
152,700 |
1.633 |
|
|
PP230K |
231,300 |
41,800 |
150,000 |
1.481 |
|
|
PP210K |
210,000 |
41,200 |
137,900 |
1.397 |
|
|
PP200K |
197,100 |
40,600 |
131,000 |
1.28 |
|
|
PP180K |
177,100 |
40,000 |
118,300 |
1.244 |
|
|
PP150K |
151,900 |
38,400 |
106,800 |
1.119 |
|
|
PP135K |
136,500 |
37,000 |
101,500 |
1 |
|
|
PP110K |
110,500 |
34,000 |
87,100 |
0.922 |
|
|
PP105K |
108,000 |
32,500 |
82,800 |
0.869 |
|
|
PP95K |
95,400 |
28,100 |
72,500 |
0.846 |
|
|
PP60K |
59,300 |
24,700 |
52,300 |
0.605 |
|
|
PP50K |
50,400 |
23,600 |
49,700 |
0.58 |
|
|
PP45K |
47,500 |
21,300 |
42,600 |
0.541 |
|
|
PP9K |
8,600 |
2,600 |
8,500 |
0.13 |
|
|
PP6K |
6,200 |
3,000 |
6,000 |
0.113 |
|
|
PP1200 |
1,220 |
885 |
1,100 |
0.032 |
|
|
PP800 |
830 |
740 |
800 |
0.025 |
|
|
PPKIT (1.0g of each standard) |
|
|
|
|
IV* 5 Intrinsic Viscosity (dL/g) in TCB at 145°C |
|
|
(a = 0.750; K = 0.000137) |
|
|
|
|
Intrinsic Viscosity and a & K values are available in Decalin at 135°C |
|
Melt index was measured at 230°C (ASTM D 1238573) using both 2.16Kg |
|
|
|
|
|
|
|
聚丙烯(Low Mw, Narrow MWD) |
|
|
|
|
货号 |
Mp |
Mw |
Mn |
IV* |
|
|
PP2700 |
2,700 |
2,850 |
2,700 |
0.057 |
|
|
PP2600 |
2,575 |
2,650 |
2,530 |
0.052 |
|
|
PP2100 |
2,100 |
2,150 |
2,020 |
0.045 |
|
|
PP1900 |
1,850 |
1,900 |
1,800 |
0.042 |
|
|
PP1800 |
1,800 |
1,770 |
1,630 |
0.039 |
|
|
PP1650 |
1,650 |
1,660 |
1,575 |
0.037 |
|
|
PP1450 |
1,450 |
1,440 |
1,375 |
0.033 |
|
|
PP1365 |
1,365 |
1,400 |
1,355 |
0.032 |
|
|
PP1300 |
1,300 |
1,290 |
1,230 |
0.03 |
|
|
PP1160 |
1,160 |
1,175 |
1,120 |
0.028 |
|
|
PP1075 |
1,075 |
1,100 |
1,070 |
0.027 |
|
|
PP1000 |
1,000 |
1,015 |
965 |
0.026 |
|
|
PP900 |
900 |
930 |
890 |
0.023 |
|
|
PP875 |
875 |
890 |
850 |
0.023 |
|
|
PP780 |
780 |
800 |
760 |
0.021 |
|
|
PPNRKIT (250mg of each standard) |
|
|
|
IV* 5 Intrinsic Viscosity (dL/g) in THF at 30°C |
|
|
(a = 0.78; K = 0.00014) |
|
|
|
|
|
|
|
|
|
|
| |
|